Steel Bars 0.95Cr - 0.20Mo (0.28 to 0.33C) (SAE 4130) Hardened and Tempered, 125 Ksi (862 MPa) Tensile Strength
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 15Cr - 6.5Ni - 0.75Mo - 0.30 Cb (Nb) - 1.5Cu Consumable Electrode Remelted, Solution Heat Treated Precipitation Hardenable
Automated Gaseous Nitriding Controlled by Nitriding Potential
General Requirements for Hydraulic System Reservoirs
Laser-Powder Bed Fusion (L-PBF) Produced Parts, Nickel Alloy, Corrosion and Heat-Resistant, 62Ni - 21.5Cr - 9.0Mo - 3.65Nb Stress Relieved, Hot Isostatic Pressed and Solution Annealed
Nickel Alloy, Corrosion and Heat-Resistant, Powder for Additive Manufacturing, 62Ni - 21.5Cr - 9.0Mo - 3.65Nb
Process Requirements for Production of Metal Powder Feedstock for Use in Additive Manufacturing of Aerospace Parts
Steel Bars, Forgings, and Tubing 1.7Cr - 3.8Ni - 0.3Mo (0.32 - 0.38C) Aircraft-Quality
Steel Bars, Forgings, and Tubing 1.0Cr - 3.2Ni - 0.2Mo (0.12 - 0.17C) Aircraft-Quality